# WELDING PROCEDURE SPECIFICATION (WPS) QW-482 (Front)

WPS No.: ____  
Date ____  
Support PQR No. (s) ____  
Revision No. ____  
Date ____  
By: ____

Welding Process: _____  
Type(s): _____

(Automatic, Manual, Machine, or Semi-Auto)

## JOINTS (QW-402)

| JOINTS (QW-402)                    |   |
|-------------------------------------|---|
| Joint Design                        |   |
| Backing(Yes)_(No)                  |   |
| Backing Material(Type)              |   |
| (Refer to both backing and retainers)|   |
| ☐ Metal                             |   |
| ☐ Nonfusing Metal                   |   |
| ☐ Nonmetallic                       |   |
| ☐ Other                             |   |

Sketches, Production Drawings, Weld Symbols or Written Description should show the general arrangement of the parts to be welded. Where applicable, the root spacing and the details of weld groove may be specified. (At the option of the Mfrgr., sketches may be attached to illustrate joint design, weld layers and bead sequence, e.g. for notch toughness procedures, for multiple process procedures, etc)

*BASE METALS (QW-403)

P-No. ____  
Group No. ____ to P-No ____  
Group No. ____

Specification type and grade ____ to Specification type and grade ____  
Chem. Analysis and Mech. Prop. ____ to Chem. Analysis and Mech. Prop ____  
Base Metal: Groove____ Fillet ____  
Pipe Dia. Range: Groove____ Fillet ____  
Other ____

* Each base metal-filler metal combination should be recorded individually.

---

# QW-482 (Back)

WPS No. ____  
Rev. ____

## POSITION(QW-405)

| Position(s) of Groove              |   |   |
|-------------------------------------|---|---|
| Welding Progression: Up Down        |   |   |
| Position(s) of Fillet               |   |   |

## POSTWELD HEAT TREATMENT(QW-407)

| Temperature Range | Time Range |   |   |   |   |   |
|-------------------|------------|---|---|---|---|---|

## PREHEAT(QW-406)

| PreheatTemp Min        | InterpassTemp Max | PreheatMaintenance    |   |   |
|------------------------|------------------|-----------------------|---|---|

## GAS(QW-408)

| Percent Composition   | Gas(es)(Mixture) | Flow Rate | Shielding | Trailing | Backing |
|-----------------------|------------------|-----------|-----------|---------|--------|

## ELECTRICAL CHARACTERISTICS(QW-409)

| CurrentAC或DCPolarity | Amps(Range)  | Volts(Range) |   |   |   |   |   |
|------------------------|---------------|--------------|---|---|---|---|---|

(Amps and volts range should be recorded for each electrode size, position, and thickness, etc. This information may be listed in a tabular form similar to that shown below)

| Tungsten Electrode Size and Type(Pure Tungsten, 2% Thoriated, etc.) | Mode of Metal Transfer for GMAW (Spray arc, short circuiting arc, etc.) | Electrode Wire feed speed range |   |   |   |
|-----------------------------------------------------------------------|--------------------------------------------------------------------------|---------------------------------|---|---|---|

## TECHNIQUE(QW-410)

| String or Weave Bead  | Orifice or Gas Cup Size | Initial and Interpass Cleaning(Brushing, Grinding, etc.) | Method of Back Gouging | Oscillation | Contact Tube to Work Distance | Multiple or Single Pass(per side) | Multiple or Single Electrodes | Travel Speed(Range) | Peening | Other |
|------------------------|------------------------|---------------------------------------------------|--------------------|------------|-------------------------|----------------------------------|--------------------------|-------------------|--------|------|

## Weld Layer(s)

| Process | Filler Metal |   | Current |   | Volt Range | Travel Speed Range | Other(e.g. Remarks, Comments, Hot Wire Addition, Technique, Torch Angle, etc.) |
|---------|--------------|---|---------|---|------------|--------------------|---------------------------------------------------------------|

| Weld Layer(s) | Process | Class | Dia | Type Polar | Amp Range | Volt Range | Travel Speed Range | Other(e.g. Remarks, Comments, Hot Wire Addition, Technique, Torch Angle, etc.) |
|---------------|--------|-------|-----|------------|-----------|------------|-------------------|-----------------------------------------------------------|
|               |        |       |     |            |           |            |                   |                                                           |